CMS specializes in precision CNC machining of PTFE components for applications requiring exceptional chemical resistance, low friction, and high-temperature performance. With advanced turning, milling, and Swiss machining capabilities, we produce high-accuracy PTFE parts such as seals, valve seats, insulators, spacers, and chemical-handling components. Our optimized processes ensure stable dimensions, clean surfaces, and consistent quality despite PTFE’s softness and deformation tendencies. From prototypes to production, CMS delivers fast lead times and ISO-certified reliability.
Start your PTFE CNC machining project today—upload your CAD files for an instant quote.
Recently CNC Machined PTFE(Teflon) Parts
Why Choose CMS for CNC PTFE Machining?
PTFE Material Properties
| Property | Value |
|---|---|
| Density | 2.2 g/cm³ |
| Hardness | Shore D 50–60 |
| Tensile Strength | 20–30 MPa |
| Continuous Service Temp | 260°C |
| Friction Coefficient | Extremely low |
| Chemical Resistance | Excellent (nearly inert) |
| Electrical Insulation | Outstanding |
| Moisture Absorption | Near zero |
PTFE is one of the most chemically inert and friction-resistant plastics available.

Our CNC ABS Machining Capabilities
Processes
- CNC turning (ideal for rings, seals, bushings)
- CNC milling (complex blocks, manifolds, insulators)
- Threading, boring, pocketing
- Ultrasonic cleaning
- Assembly machining with inserts or bonded components
Tolerance Standards
- PTFE is soft and compressible, so tolerances differ from hard plastics:
- Standard: ±0.10 mm
- Precision: ±0.05 mm (depends on geometry and wall thickness)
- Surface finish: Ra 1.6–3.2 μm
Frequently Question
If you have any questions in the process of product design and manufacturing, you can contact us to obtain expert support and provide the best solution for your product. Get support now !
client
testimonials

Supplier was very helpful througout the whole process and very easy to communicate with, the end product turned out great with good anodizing quality and overall quality.
Edward Kinsjer
It All Starts With a consultation!
PTFE(Teflon) Parts CNC Machining Service
For any kind of quiries, Please Email
Room 902, Building 37, Gaoao New Village, Longhua District, Shenzhen City, Guangdong Province, China. 518100
+8617196430663