CNC PE Machining Service (HDPE / UHMWPE / PE500 / PE1000)
Precision CNC machining for polyethylene components with excellent impact resistance, wear performance, and chemical stability—ideal for industrial, mechanical, and food-grade applications.
1. No MOQ
2. Start as low as $1
3. Fastest 3 days delivery
4.7*24H free quotation and technical support

Polyethylene (PE) CNC Machining Service Supplier in China
CMS provides reliable and precise CNC machining for polyethylene (PE) components, including HDPE, UHMWPE, PE500, and PE1000. With advanced milling and turning capabilities, we produce tough, wear-resistant, and chemically stable PE parts for industrial machinery, food processing, marine applications, and conveyor systems. Our machining strategies ensure clean edges, accurate dimensions, and consistent performance despite PE’s softness and flexibility. From prototypes to mass production, CMS delivers fast lead times and dependable quality.
Start your CNC PE machining project today—upload your CAD files for an instant quote.
Recently CNC Machined Polyethylene (PE) Parts
Why Choose CMS for CNC PE Machining?
PE Material Properties
| Property | HDPE | UHMWPE (PE1000) |
|---|---|---|
| Density | 0.95 g/cm³ | 0.93–0.94 g/cm³ |
| Tensile Strength | ~25 MPa | ~20 MPa |
| Hardness | Shore D 65–70 | Shore D 60–65 |
| Wear Resistance | Good | Excellent |
| Impact Resistance | High | Extremely high |
| Moisture Absorption | Near zero | Near zero |
| Chemical Resistance | Excellent | Excellent |

Our CNC ABS Machining Capabilities
Processes
- CNC milling (3-axis & 5-axis)
- CNC turning
- Contouring, slotting, pocketing
- Boring, drilling, tapping
- Machining of large plastic plates/blocks
Tolerance Standards
PE is flexible and hard to fixture, so tolerances differ from rigid plastics:
- Standard: ±0.10–0.20 mm
- Precision: ±0.05–0.10 mm (case-dependent)
- Surface finish: Ra 1.6–3.2 μm
Frequently Question
If you have any questions in the process of product design and manufacturing, you can contact us to obtain expert support and provide the best solution for your product. Get support now !
client
testimonials

Supplier was very helpful througout the whole process and very easy to communicate with, the end product turned out great with good anodizing quality and overall quality.
Edward Kinsjer
It All Starts With a consultation!
Polyethylene (PE) Parts CNC Machining Service
For any kind of quiries, Please Email
Room 902, Building 37, Gaoao New Village, Longhua District, Shenzhen City, Guangdong Province, China. 518100
+8617196430663