Quick Answer: CNC machining aluminum parts requires matching the alloy grade to the dominant application requirement, not selecting based on strength alone. 6061-T6 is the default choice for approximately 70% of CNC aluminum applications, providing the best balance of machinability, moderate strength (~250–300 MPa), and corrosion resistance. 7075-T6 provides approximately double the strength (~450–550 MPa) for weight-critical structural applications at higher cost, reduced corrosion resistance, and more difficult machining. 2024 provides superior fatigue resistance for cyclically loaded aerospace structures but has poor corrosion resistance without coating. 5052 is optimized for sheet-forming applications, not CNC machining. Beyond alloy selection, achievable precision in aluminum is governed primarily by deformation control — aluminum’s relatively low elastic modulus (~70 GPa, roughly one-third of steel) makes wall thickness, fixturing, and machining sequence the dominant factors determining whether a part holds tolerance, not raw machine accuracy. Typical achievable tolerance in well-controlled aluminum CNC machining is ±0.05 mm general, ±0.01–0.02 mm on precision features, and ≤0.05 mm flatness on plates using stress-relieved material.


Why Aluminum Dominates CNC Machining Across Industries

Aluminum’s prevalence in CNC machining stems from a combination of properties that together produce the best overall manufacturing efficiency among common engineering metals — not from being the strongest, lightest, or cheapest material in isolation.

Strength-to-weight ratio: At a density of approximately 2.7 g/cm³ (roughly one-third of steel’s 7.85 g/cm³), aluminum alloys like 6061-T6 (yield strength ~250–300 MPa) provide sufficient structural strength for the majority of mechanical components at a fraction of steel’s weight — directly relevant for aerospace, robotics, automotive, and any application where mass reduction improves performance or efficiency.

Machinability: Aluminum’s low cutting forces allow cutting speeds 2–5× higher than steel with excellent chip evacuation, producing faster cycle times, longer tool life, and lower per-part machining cost. This machinability advantage is frequently the larger economic factor compared to raw material cost differences between aluminum and other metals.

Natural corrosion resistance: Aluminum forms a protective aluminum oxide (Al₂O₃) layer naturally, providing corrosion resistance adequate for many outdoor and general industrial environments without additional coating — though this natural oxide layer is thinner and less durable than the engineered anodized layer typically specified for functional or cosmetic applications.

Finishing compatibility: Aluminum’s compatibility with anodizing (Type II and Type III/hard anodize), powder coating, and mechanical polishing provides more finishing flexibility than most engineering metals, supporting both functional surface requirements (wear resistance, electrical insulation) and cosmetic requirements within the same base material.

Rapid iteration capability: Combined with low tool wear and easy reworkability, these properties make aluminum particularly well-suited to prototyping and low-to-medium volume production where design iteration speed matters as much as final part performance.


Aluminum Grade Selection Guide

Grade Yield Strength Machinability Corrosion Resistance Key Advantage Primary Limitation
6061-T6 ~250–300 MPa Excellent Good Balanced performance, versatile, default choice Not the highest-strength option
7075-T6 ~450–550 MPa Moderate Lower Very high strength-to-weight ratio Higher cost, lower corrosion resistance, more difficult machining
2024 ~400–470 MPa Moderate Poor (requires coating) Excellent fatigue resistance Poor corrosion resistance without protective coating
5052 ~150–250 MPa Poor for CNC Excellent High ductility, ideal for forming Not optimized for CNC machining
MIC-6 (cast tooling plate) ~150–200 MPa Excellent Good Exceptional flatness and dimensional stability Lower strength than wrought alloys

6061-T6 as the default choice: For general CNC machined parts without an extreme strength, fatigue, or forming requirement, 6061-T6 provides the best combination of machinability, adequate strength, and corrosion resistance. When the application requirement is unclear or has no specific driver toward a specialized grade, 6061-T6 is the correct starting point — it covers the majority of structural and mechanical component applications.

7075-T6 for strength-critical, weight-sensitive applications: When 6061’s strength is insufficient and the application specifically requires the higher strength-to-weight ratio that 7075 provides — aerospace brackets, high-load structural components — the trade-offs (higher material and machining cost, reduced corrosion resistance, more demanding machining parameters) are justified by the functional requirement. Specifying 7075 “for extra strength” when 6061 would meet the actual load requirement is a common source of avoidable cost.

2024 for fatigue-critical, cyclically loaded structures: 2024’s superior fatigue performance under cyclic loading makes it the standard choice for aerospace fatigue-critical structures — but its corrosion resistance is poor enough that protective cladding or coating is typically required for any application with environmental exposure. This alloy should be reserved specifically for fatigue-dominant load cases, not general structural use.

5052 for forming, not CNC machining: 5052’s value proposition (high ductility, excellent corrosion resistance) is specifically relevant to sheet metal forming and bending operations — it is not optimized for CNC machining and should not be specified for machined parts unless the application specifically requires its formability characteristics elsewhere in the part’s manufacturing sequence.

MIC-6 for flatness-critical precision plates: MIC-6 is a stress-relieved cast tooling plate specifically engineered for dimensional stability — minimal warping during machining due to its controlled internal stress state. For base plates, fixtures, and precision flat components requiring flatness tighter than approximately 0.05 mm, MIC-6 provides reliability that standard wrought aluminum plate, with its inherent rolling-induced internal stress, cannot match as consistently.


Common DFM Mistakes That Cause Aluminum Parts to Fail Tolerance

Most aluminum CNC machining failures originate from applying design rules developed for steel without accounting for aluminum’s lower stiffness and higher relative ductility.

Thin wall deformation: Aluminum’s elastic modulus (~70 GPa) is roughly one-third of steel’s (~200 GPa), meaning aluminum walls deflect approximately 3× more than geometrically identical steel walls under equivalent cutting or clamping force. The deflection during machining produces dimensional inaccuracy, chatter marks from vibration, and post-machining springback as the part relaxes after fixture release. The design rule: minimum wall thickness of ≥1.5 mm for general features, increasing to ≥2.0–3.0 mm for unsupported or cantilevered features.

Deep pocket tool deflection: Deep cavities require long, slender end mills that deflect under cutting load proportionally to the cube of their length — producing tapered walls, degraded surface finish, and dimensional error concentrated at the pocket bottom. The standard design guideline limits depth-to-width ratio to approximately 3–4:1 for pockets machined with standard tooling; deeper features require specialized tooling or alternative machining strategies.

Sharp internal corners: CNC end mills are round tools and cannot produce a true sharp (zero-radius) internal corner — attempting to specify one leaves residual material at the corner or requires secondary processing. Specifying an internal corner radius of at least 0.5–1.0 mm (matched to available tool diameter) avoids this manufacturability conflict and reduces both machining time and cost compared to attempting to approximate a sharp corner.

Poor tool access: Complex geometries that block straightforward tool paths — deep internal features reachable only from awkward angles, undercuts requiring tool reorientation — increase tool changes, cycle time, and surface quality variability. Designing features aligned with standard tool approach directions (vertical access for 3-axis machining, or planned multi-axis access for 5-axis capability) avoids unplanned machining complexity discovered only after the part reaches the CNC programming stage.

Tolerance over-specification: Applying unnecessarily tight tolerances (e.g., ±0.01 mm) across an entire part rather than only on functionally critical features dramatically increases machining time, scrap rate, and inspection cost without corresponding functional benefit. The practical guideline: general non-functional features at ±0.05–0.10 mm, with tighter tolerance reserved specifically for features where fit, alignment, or sealing function requires it.


Controlling Tolerance, Flatness, and Deformation

Achievable precision in aluminum CNC machining is governed by deformation control throughout the process — material selection, machining sequence, fixturing, and thermal management — not solely by the CNC machine’s positioning accuracy.

Residual stress management: Rolled or extruded aluminum stock contains internal stress from the manufacturing process. As material is removed during machining, these stresses redistribute, causing the part to warp progressively as machining proceeds — sometimes becoming apparent only after the part is removed from the fixture. Using stress-relieved material (T651 temper, or MIC-6 for plate applications) and incorporating a rough-machine, rest, finish-machine sequence (allowing the part to relax between roughing and final dimensional passes) are the standard mitigation strategies.

Machining sequence planning: Removing material asymmetrically creates an imbalanced internal stress distribution that causes the part to bend or twist mid-process. Symmetric material removal strategy, a defined roughing-semi-finishing-finishing sequence, and leaving approximately 0.2–0.5 mm of stock for the final finishing pass (removing the material affected by earlier-stage stress redistribution) all contribute to dimensional stability through the complete machining sequence.

Fixture design: Excessive mechanical clamping force deforms aluminum’s relatively low-stiffness sections, and the part springs back toward its unconstrained shape after the fixture releases — producing dimensional results that measure differently in the fixture versus after the part is removed. Low clamping force, distributed support across the part’s bearing surfaces, and vacuum fixtures (particularly effective for thin plates) maintain part shape without introducing the deformation that aggressive mechanical clamping causes.

Thermal expansion: Aluminum’s coefficient of thermal expansion (~23 µm/m·°C) is approximately double that of steel, meaning ambient temperature variation in the shop environment produces measurably larger dimensional shift in aluminum parts during machining and inspection. Maintaining stable shop temperature and allowing parts to thermally equilibrate before final dimensional inspection are necessary for high-precision aluminum work — a 5°C temperature swing on a 200 mm aluminum part produces approximately 0.023 mm dimensional change, which can exceed the tolerance band for precision features.

Achievable tolerance capability with proper process control:

Feature Type Typical Capability Risk Level
General dimensions ±0.05–0.10 mm Low
Precision fits ±0.01–0.02 mm Medium
Thin walls ±0.05 mm+ variation possible High
Flatness (plates) ≤0.05 mm (with stress-relieved material) Medium–high
Deep pockets ±0.05–0.10 mm High

Surface Finishing Options

Process Typical Thickness Hardness Corrosion Resistance Electrical Conductivity Typical Application
Anodizing (Type II) 5–25 µm Medium High Insulating General-purpose protection and color
Hard anodizing (Type III) 25–75 µm High (~400–600 HV) Very high Insulating Wear and sliding surfaces
Bead blasting N/A (surface texture only) N/A None alone Conductive Surface prep before coating; cosmetic uniformity
Chromate conversion (Alodine) 0.5–2 µm Low Moderate Conductive Electrical grounding, aerospace assemblies
Powder coating 50–150 µm Medium High Insulating Outdoor and cosmetic housings (non-precision)

Anodizing’s dimensional effect must be designed for: Anodizing converts the surface aluminum into aluminum oxide, with the resulting layer building both into and out of the original surface — approximately half the coating thickness penetrates inward (consuming base material) and half builds outward. For a Type II anodize at 15 µm, this means approximately 7.5 µm of outward dimensional growth on each surface — relevant for any threaded feature, precision fit, or critical clearance that must accommodate this buildup. Hard anodizing’s substantially greater thickness (25–75 µm) makes this dimensional allowance even more critical to incorporate during the design phase, not after the part is machined to its “final” dimension.

Selecting by function, not appearance alone: Anodizing (Type II) is the default choice for general corrosion protection and color options. Hard anodizing is reserved for surfaces specifically requiring wear resistance, given its higher cost and greater dimensional impact. Chromate conversion is specified when electrical conductivity must be maintained — anodizing’s insulating oxide layer makes it unsuitable for electrical grounding or RF shielding contact surfaces. Powder coating provides the thickest protective layer for outdoor cosmetic housings but its limited dimensional control makes it unsuitable for tight-tolerance functional features.


Cost Drivers in CNC Machining Aluminum

Material price is rarely the dominant cost factor in CNC aluminum machining — geometry complexity and machining time typically account for the majority of total part cost.

Typical cost contribution breakdown: Material cost: 10–30%; machining time: 40–60% (the largest single driver); setup and programming: 10–20%; finishing and inspection: 10–20%. This distribution means that design decisions affecting machining time — geometry complexity, wall thickness, pocket depth, and tolerance specification — have substantially more cost impact than the choice between 6061 and a more expensive alloy.

Machining time as the dominant lever: Deep pockets, thin walls (requiring slower, lighter cutting passes to avoid deflection), tight tolerances (requiring additional finishing passes and verification), and complex toolpaths all directly increase cycle time. Reducing machining time through geometry simplification is consistently the most effective cost reduction strategy, more impactful than material substitution in most cases.

Setup cost dominates at low volume: Programming (CAM toolpath generation), fixture design and fabrication, and machine setup represent a largely fixed cost per part design, regardless of batch size. This fixed cost is amortized across the batch quantity, meaning unit cost drops rapidly from prototype quantities (1–10 pieces, highest unit cost) through small batch (10–100 pieces, unit cost dropping significantly) to production volumes (100+ pieces, optimized pricing) — primarily due to setup cost amortization rather than any change in the per-part machining operation itself.

Surface finishing adds 10–30% to total part cost: Anodizing, hard anodizing, and powder coating each add processing cost, handling risk, and — as discussed above — dimensional changes that must be accounted for in design. This cost should be incorporated into total part cost comparisons from the earliest design stage, not treated as an afterthought once machining is complete.


Tolerance Is Frequently the Single Largest Cost Multiplier

While material grade and geometry both affect cost, tolerance specification is frequently the single factor most responsible for unplanned cost escalation — because tightening tolerance does not increase cost linearly; it increases the requirements for cutting speed, finishing passes, fixturing rigidity, and inspection method simultaneously.

Tolerance Relative Cost What Changes in Manufacturing
±0.1 mm Low (baseline) Standard machining parameters, fast cycle time, simple gauge inspection
±0.05 mm Medium Controlled machining parameters, basic dimensional inspection
±0.02 mm High Slower feeds, additional finishing passes, CMM verification typically required
±0.01 mm Very high Precision setup, multiple finishing passes, strict environmental and inspection control

The critical design principle is feature-specific tolerance allocation, not part-wide tolerance specification. Most parts have only a small number of features where tight tolerance is functionally necessary (a bearing bore, a sealing face, a mating alignment feature) — applying the tightest required tolerance to every dimension on the part, rather than identifying and tightening only the functionally critical features, is one of the most common and most expensive specification mistakes in aluminum CNC machining. A housing with only its bearing bore held to ±0.01 mm (with the remainder of the part at ±0.05 mm) achieves the same functional outcome as a part held to ±0.01 mm everywhere, at substantially lower cost.

Industry-typical tolerance ranges illustrate that tolerance is function-driven, not industry-driven:

Industry/Application Context Typical Tolerance Range Critical Features (where tight tolerance actually applies)
Consumer electronics ±0.05–0.1 mm Cosmetic alignment surfaces, mating edges
Robotics ±0.02–0.05 mm Mounting interfaces, joint alignment features
Aerospace ±0.005–0.02 mm Load-bearing and mating structural features specifically
Automotive ±0.02–0.05 mm Functional engine/assembly interfaces
General industrial equipment ±0.05–0.1 mm Mounting and general structural features

The pattern across every industry listed is the same: only a specific subset of features within the part actually require the tighter end of the industry’s typical range — the common mistake is assuming an industry label (“aerospace,” “robotics”) implies the entire part requires the tightest tolerance associated with that industry, when in practice even aerospace components hold the majority of non-critical dimensions to comparatively standard tolerance and reserve ultra-tight tolerance specifically for the structural or mating features where it is functionally required.


CNC Machining vs Die Casting, Extrusion, and Sheet Metal Fabrication

Factor CNC Machining Die Casting Extrusion Sheet Metal
Precision Highest Moderate Lower Lower–moderate
Geometry complexity capability Highest (full 3D) High Limited to constant cross-section Moderate (2.5D forming)
Tooling cost Very low (no dedicated tooling) Very high High Moderate
Volume efficiency Lower (cost doesn’t improve dramatically at scale) Excellent at high volume Excellent at high volume Good
Design flexibility Highest (any design change is just a program edit) Lowest (requires new tooling for changes) Limited to extrudable profile changes Moderate

CNC machining is preferred for low-to-medium volume (typically below approximately 5,000 pieces), tight tolerances (±0.01–0.02 mm), or designs still under development where the absence of tooling investment provides both cost advantage and the flexibility to accommodate design changes without re-tooling cost.

Die casting becomes economical at high volume with stable geometry, once the very high tooling investment ($10,000–$100,000+ depending on complexity) is amortized across a large production run — typically above 5,000–10,000 pieces for the economics to favor casting over CNC.

Extrusion is limited to constant cross-section profiles but is highly efficient for parts that match this geometric constraint. A common hybrid strategy extrudes the basic profile and uses CNC machining to add features (holes, slots, complex end geometry) that the extrusion process cannot produce — combining extrusion’s volume efficiency with CNC’s geometric flexibility for the features that require it.

Sheet metal fabrication is preferred for thin, formed parts (typically below 6–8 mm thickness) where bending and forming operations efficiently produce the required geometry; CNC machining becomes preferable as part thickness increases and 3D geometric complexity (pockets, complex internal features) exceeds what forming can achieve.


Scaling from Prototype to Production

Scaling successfully from a working prototype to stable, repeatable production requires controlling variation, not simply running the same process at higher volume.

Repeatability is the foundation: A prototype that worked once does not guarantee a repeatable process. Tool wear variation, fixture inconsistency, and operator-to-operator differences all introduce variation that becomes problematic at production scale. Locking cutting parameters, toolpaths, and setup procedures into a documented, standardized process is the necessary first step before scaling volume.

Statistical Process Control (SPC): Monitoring dimensional variation in real time through sampling inspection and control charts allows drift to be detected and corrected before parts go out of tolerance. The standard process capability targets are Cpk ≥ 1.33 for general production and Cpk ≥ 1.67 for high-precision applications; a Cpk below 1.0 indicates a process at high risk of producing out-of-tolerance parts even under nominal operation.

Fixture standardization: Inconsistent clamping between setups is a primary source of dimensional variation at scale. Dedicated fixtures with repeatable locating features — and vacuum fixtures specifically for thin aluminum parts prone to clamping-induced distortion — define repeatability more directly than the machine’s inherent positioning accuracy does.

Automation opportunities: Tool changes, part loading/unloading, and in-process measurement are common automation targets that reduce human-introduced variation and increase throughput as production volume justifies the automation investment — typically becoming economically relevant above medium production volumes where the automation cost can be amortized across sufficient parts.


Real Application Examples

Application Dominant Requirement Material Process Strategy Result
Aerospace bracket Strength-to-weight ratio 7075-T6 Precision 5-axis CNC ~2× strength vs 6061; weight reduction maintained at ±0.02 mm tolerance
UAV structural frame Lightweight + fatigue/vibration 6061-T6 (with ribbed structure) High-speed CNC with geometric stiffening Optimized weight-to-rigidity without 7075’s cost premium
Robotic housing Complex geometry + thermal + appearance 6061-T6 CNC + bead blasting + anodizing Combined thermal performance, surface finish, and cost control
Electronics enclosure Flatness + thermal + EMI 6061-T6 or MIC-6 (flat panels) CNC + anodizing Stable flatness (≤0.05 mm) for consistent assembly fit
Medical equipment component Precision + repeatability + corrosion 6061-T6 CNC + controlled anodizing Stable ±0.01–0.02 mm tolerance with scalable, repeatable process

The consistent pattern across applications: The aerospace bracket case demonstrates that 7075 is selected only when strength is the genuinely limiting factor, not as a default upgrade. The UAV frame case demonstrates that geometric optimization (ribbed structure for stiffness) frequently substitutes for a more expensive alloy upgrade — addressing the functional requirement (stiffness) through design rather than material cost. These cases illustrate that material selection alone does not determine project success; DFM design, process control, and manufacturing strategy contribute equally to the outcome.


Key Takeaways

  • 6061-T6 is the correct default alloy for approximately 70% of CNC aluminum applications: it provides the best balance of machinability, adequate strength, and corrosion resistance. Reserve 7075-T6 for genuine strength-to-weight requirements, 2024 for fatigue-dominant cyclic loading, and MIC-6 for flatness-critical precision plates.
  • Aluminum’s lower elastic modulus (~70 GPa vs steel’s ~200 GPa) makes deformation control, not raw machine accuracy, the limiting factor for precision: minimum wall thickness (≥1.5 mm general, ≥2.0–3.0 mm unsupported), controlled clamping force, and proper machining sequence (rough → rest → finish) are necessary for tolerance-critical parts.
  • Residual stress in rolled or extruded aluminum stock causes warping as material is removed during machining: using stress-relieved material (MIC-6, T651 temper) and a structured roughing-to-finishing sequence with stock allowance for the final pass mitigates this dimensional risk.
  • Anodizing changes part dimensions and must be incorporated into design tolerances: approximately half the coating thickness builds outward on the surface (Type II: 5–25 µm; hard anodize: 25–75 µm), directly affecting threaded features, precision fits, and critical clearances.
  • Machining time, not material price, dominates total part cost: typically 40–60% of total cost versus 10–30% for raw material. Geometry simplification — reducing pocket depth, avoiding unnecessary thin walls, relaxing non-functional tolerances — is consistently the most effective cost reduction strategy.
  • CNC machining is the correct process for low-to-medium volume (below ~5,000 pieces), tight tolerances, or evolving designs: die casting becomes economical only once tooling investment is amortized across high volume (typically 5,000–10,000+ pieces with stable geometry).
  • For OEM procurement and design teams: aluminum CNC drawings should specify the exact alloy and temper (e.g., “6061-T6 per ASTM B221,” not just “aluminum”), distinguish functionally critical tolerances from general dimensions explicitly, and specify any post-machining surface treatment with its dimensional allowance accounted for in the base machined dimension — not added as an assumption after the drawing is finalized.

Frequently Asked Questions

What is the best aluminum alloy for CNC machining?

6061-T6 is the best all-around aluminum alloy for CNC machining, covering approximately 70% of applications due to its excellent machinability, adequate strength (~250–300 MPa yield), and good corrosion resistance at relatively low cost. Exceptions apply when a specific requirement dominates: 7075-T6 for applications requiring approximately double 6061’s strength-to-weight ratio (aerospace, high-load structures); 2024 for fatigue-critical cyclic loading applications (with the trade-off of poor corrosion resistance requiring protective coating); and MIC-6 cast tooling plate for applications requiring exceptional flatness and dimensional stability (precision fixtures, base plates). The selection should be driven by the application’s dominant requirement, not by defaulting to the highest-strength option available.

What tolerances can CNC machined aluminum parts achieve?

Well-controlled aluminum CNC machining typically achieves ±0.05–0.10 mm on general dimensions, ±0.01–0.02 mm on precision features with appropriate process control, and ≤0.05 mm flatness on plates using stress-relieved material such as MIC-6. These tolerances are limited primarily by deformation control rather than raw CNC machine positioning accuracy — aluminum’s relatively low elastic modulus (~70 GPa, about one-third of steel) means that wall thickness, clamping force, residual stress in the stock material, and thermal expansion during machining and inspection all directly affect whether a part holds its design tolerance. Thin walls and deep pockets carry the highest risk of tolerance variation, often exceeding ±0.05 mm without specific design and process accommodation.

Does anodizing affect the dimensions of CNC machined aluminum parts?

Yes, significantly. Anodizing converts surface aluminum into aluminum oxide, with the resulting coating building both inward (consuming base material) and outward (adding surface thickness) — approximately half the total coating thickness in each direction. Type II anodizing (5–25 µm typical thickness) and hard anodizing (Type III, 25–75 µm) both produce measurable outward dimensional growth that must be accounted for in the design of threaded features, precision fits, and critical clearances. A part machined to its “final” dimension without accounting for anodizing buildup will be measurably oversized on external features and undersized on internal features after coating — a common and avoidable design oversight.

How can thin-wall deformation be prevented in aluminum CNC machining?

Thin-wall deformation, the most common precision issue in aluminum machining, is addressed through several complementary strategies: increasing minimum wall thickness to ≥1.5–2.0 mm for general features (≥2.0–3.0 mm for unsupported or cantilevered sections); using low clamping force with distributed support, including vacuum fixtures for thin plates, to avoid the mechanical deformation that aggressive clamping introduces; optimizing the machining sequence (rough machining, allowing the part to relax, then finish machining) to manage residual stress redistribution as material is removed; and selecting stress-relieved material where flatness is particularly critical. Design and fixturing strategy generally have more influence on thin-wall outcome than cutting parameter optimization alone.

When should aluminum parts be cast instead of CNC machined?

Die casting becomes the more economical choice when production volume exceeds approximately 5,000–10,000 pieces and the part geometry is stable (not expected to change during the production run), because the very high tooling investment ($10,000–$100,000+ depending on complexity) is amortized across the large volume, producing a lower per-part cost than CNC machining’s continued machining time cost at that volume. Below this volume threshold, or for parts with design changes still likely, CNC machining remains more economical because it requires no tooling investment and can accommodate design revisions as simple program edits rather than new tooling. A common hybrid strategy uses die casting (or extrusion) for the basic part geometry and CNC machining for precision features that the casting or extrusion process cannot produce to the required tolerance — combining the volume economics of one process with the precision capability of the other.


Written by the CMS engineering team with 15+ years of CNC machining experience producing aluminum components in 6061-T6, 7075-T6, 2024, 5052, and MIC-6 for aerospace, UAV, robotics, electronics, and medical device OEM manufacturing programs — including DFM review, deformation control strategy, and surface finishing coordination from prototype through production scaling. Technical references: ASTM B221 (Aluminum Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes), ASTM B209 (Aluminum and Aluminum-Alloy Sheet and Plate), MIL-A-8625 (Anodic Coatings for Aluminum), ASM Handbook Vol. 2 (Properties and Selection — Nonferrous Alloys, Aluminum and Aluminum Alloys chapter), Kaufman J.G. — Introduction to Aluminum Alloys and Tempers (ASM International).


Sourcing CNC Machined Aluminum Components?

At CMS, we produce precision CNC machined aluminum parts in 6061, 7075, 2024, and MIC-6 — from prototype through production scaling, with deformation-aware DFM review, anodizing coordination with dimensional allowance calculation, and CMM first-article dimensional inspection.

[Request an aluminum CNC machining specification review and quote →]
post contents

Contact Info

Get the latest news & updates

subscribe to our newsletter