Bronze CNC Machining Service Supplier in China
CMS provides high-precision CNC machining for bronze components requiring exceptional wear resistance, strength, and corrosion performance. With advanced milling, turning, and Swiss machining capabilities, we produce reliable bronze parts such as bushings, bearings, gears, and valve components. From prototypes to large-volume production, our team ensures consistent quality, smooth finishes, and competitive pricing—without any minimum order quantity.
Start your CNC bronze machining project today—upload your CAD files for an instant quote.
Cases of CNC Bronze Parts
Why Choose CMS for CNC Bronze Machining?
Bronze Materials We Work With
| Bronze Grade | Key Features | Density (g/cm³) | Yield Strength (MPa) | Hardness (HB) | Typical Applications |
|---|---|---|---|---|---|
| C93200 | Excellent wear resistance (bearing bronze) | 8.7–8.9 | 130–200 | HB 65–80 | Bushings, bearings, wear plates |
| C95400 | High strength, corrosion resistance (aluminum bronze) | 7.6–7.7 | 350–500 | HB 170–190 | Gears, heavy-duty parts, valves |
| C65500 | High corrosion resistance, good formability (silicon bronze) | 8.3–8.5 | 275–350 | HB 95–120 | Marine hardware, fasteners |
Features of CNC Machining Bronze Parts
– Bronze parts and assemblies provide a tighter seal for fittings
– Can reduce production costs and is very strong under high stress
– Can withstand extreme temperatures
– easy to cast
– High heat and corrosion resistance, rust resistance and more premium properties
– Extremely durable and long service life
– Lightweight and easy to carry or install

Frequently Question
If you have any questions in the process of product design and manufacturing, you can contact us to obtain expert support and provide the best solution for your product. Get support now !
client
testimonials

Supplier was very helpful througout the whole process and very easy to communicate with, the end product turned out great with good anodizing quality and overall quality.
Edward Kinsjer
It All Starts With a consultation!
Bronze Parts CNC Machining Service
For any kind of quiries, Please Email
Room 902, Building 37, Gaoao New Village, Longhua District, Shenzhen City, Guangdong Province, China. 518100
+8617196430663